Painting in cold and damp: how to apply cold galvanizing in winter
In winter many jobs stop for a simple reason: almost all paints need more than 5 °C to dry properly. If you apply in the cold, the paint stays soft for days, traps moisture and fails early. For those who work outdoors, that means weeks lost.
GALVANOL works in the cold
The can and pail version of GALVANOL can be applied between -30 °C and +60 °C, with relative humidity up to 90%. Touch-dry times according to its technical data sheet are:
At +20 °C: about 20 minutes.
At -10 °C: about 40 minutes.
At -30 °C: about 50 minutes.
Full drying takes about 4 hours and full cure 72 hours.
Important: the spray has a narrower range, from +5 °C to +40 °C, because it depends on propellant pressure. To work in freezing conditions, use the can or the pail.
Tips for working in winter
No ice or liquid water: GALVANOL tolerates ambient humidity, but the surface must be free of frost, ice and droplets. Dry it with a cloth or wait for the sun to dry it.
Store the product somewhere mild before use; it mixes better and flows more easily.
Mix well and stir again every 20–30 minutes: in the cold, zinc settles faster.
Work in the middle hours of the day if you can, when the surface is driest.
Respect the times between coats and don't stack coats that are too thick: several thin ones are better.
An advantage for your business
For metalworkers, installers and maintenance companies, being able to keep working in winter means invoicing doesn't stop and deliveries aren't delayed. And for industrial maintenance managers, it means making the most of December and January plant shutdowns regardless of the weather.
Work out what you need with our calculator and ask us for a quote at info@galvanol.eu.
Have a project? We are the manufacturer: write to info@galvanol.eu for quotes, samples or technical advice. Technical data sheets and safety data sheets are available in Products.