Old galvanizing with rust: how to "recharge" the zinc before it's too late
Hot-dip galvanizing is excellent protection, but it has a limited life: the zinc is gradually consumed to protect the steel. In an aggressive environment, a galvanized layer can be used up in 15–25 years. When that happens, the steel starts to rust and the structure loses value and safety.
Signs that the galvanizing is running out
White rust (whitish powder): the zinc is working. It is normal, but it shows wear.
Dull, dark areas instead of the original shine.
Red rust spots: the zinc is used up there and the steel is already corroding. This is the time to act.
Rust on bolts, welds and edges: these are usually the first points to fail.
Recharging the cathodic protection
The advantage of cold galvanizing is that it can be applied in situ, without dismantling anything or sending it to a galvanizing plant. GALVANOL is applied directly over old galvanizing, or over a surface treated years ago with GALVANOL itself, and puts zinc back into the system.
How to do it
Remove loose red rust with a wire brush or sandpaper down to sound metal.
Remove white rust and dirt; wash if there is salt or contamination.
Degrease with xylene and let dry.
Apply GALVANOL to the damaged areas and then a general coat over the whole structure. Recommended: 2 coats, or 3 in marine or industrial environments.
Why not wait?
While there is still zinc, maintenance is quick and cheap: clean and apply. Once red rust advances and pits the steel, repair is much more expensive and parts sometimes have to be replaced. Inspecting galvanized structures once a year and touching up in time multiplies their service life.
For spot touch-ups, the GALVANOL Spray 500 ml is the most convenient. For complete structures, the 10 kg pail covers about 20 m² in 2 coats.
Have a project? We are the manufacturer: write to info@galvanol.eu for quotes, samples or technical advice. Technical data sheets and safety data sheets are available in Products.