How to repair welds and cuts in galvanized steel step by step
Hot-dip galvanizing protects steel for decades, but as soon as a part is welded, cut or drilled on site, the zinc layer disappears in that area. That bare spot is where rust starts, and from there it creeps under the sound galvanizing. The good news: it can be repaired in a few minutes with a zinc-rich coating.
Why you should always repair
The heat of welding burns off the zinc a few centimetres around the bead, and spatter leaves steel exposed. The ISO 1461 and ASTM A780 standards expressly allow repair with zinc-rich paint, provided the product has enough zinc in the dry film and is applied at the right thickness.
Step by step
Let the weld cool and remove slag and spatter with a wire brush or disc.
Sand or brush down to bright steel, overlapping about 2–3 cm onto the sound galvanizing.
Degrease with xylene and let dry.
Shake well the product. If you use the spray, for at least 1 minute until you hear the ball rattle.
Apply 2 coats crosswise, letting each dry (touch-dry in about 20 min at +20 °C). For structural repair, about 105 microns dry are recommended.
Spray or can?
For spot welds, fasteners and cuts, GALVANOL Spray 500 ml is the most convenient: no mixing and no brushes to clean. For many metres of weld bead or a whole structure, a can of GALVANOL 1 kg or GALVANOL 2 kg applied by brush goes further and is more economical.
Mistakes to avoid
Painting over slag or loose rust: the zinc does not make contact with the steel.
A single thin coat: it does not reach the thickness the standard requires.
Not overlapping onto the sound galvanizing: a weak line remains right at the edge.
GALVANOL complies with ISO 1461 and ASTM A780 as a repair coating for hot-dip galvanizing, with 96% zinc in the dry film.
Have a project? We are the manufacturer: write to info@galvanol.eu for quotes, samples or technical advice. Technical data sheets and safety data sheets are available in Products.