top of page
Search

GALVANOL passes ISO 12944-6 for C4 very high and C5 high: what was tested and what it means

GALVANOL IBERIA SL
1 hour ago
3 min read

Any manufacturer can write "high corrosion resistance" on a can. What allows products to be compared is a standardised test, carried out by an independent laboratory with measurable results. In this article we explain the GALVANOL test according to UNE-EN ISO 12944-6:2018 and what each result means.

What the laboratory was asked to do

Steel panels coated with GALVANOL were tested for two combinations of corrosivity and durability from ISO 12944:

  • C4 with very high durability (VH): industrial and coastal environments with moderate salinity, with more than 25 years of expected durability.

  • C5 with high durability (H): very aggressive industrial environments and coastal areas with high salinity, with 15 to 25 years of expected durability.

For these two categories, ISO 12944-6 requires the same tests: 1,440 hours of neutral salt spray (ISO 9227) and 720 hours of continuous condensation (ISO 6270-1). The tests were carried out in an independent laboratory between February and April 2019.

Test 1: 1,440 hours of salt spray

The panels spend 60 days in a row in a chamber at 35 °C with a mist of water containing 5% salt (50 g/l sodium chloride). Beforehand, a scribe is cut through the coating down to the steel, to see what happens when the coat is damaged.

At the end, appearance is assessed according to ISO 4628, along with corrosion from the scribe. GALVANOL's result:

  • Blistering: 0(S0), none.

  • Rust: Ri 0, no rust at all on the surface.

  • Cracking: 0(S0), none.

  • Flaking: 0(S0), none.

  • Corrosion creep from the scribe: 0 mm. The standard allows up to 1.5 mm.

Test 2: 720 hours of continuous condensation

The panels spend 30 days at about 38 °C with water condensing on them non-stop, with no protection of edges or back. It simulates the permanent humidity of buildings, roofs or dew-prone areas. Result: no blistering, no rust, no cracking and no flaking (0(S0) and Ri 0 in all assessments).

Adhesion before and after

Adhesion is measured with the cross-cut test (ISO 2409): a grid of cuts is made and pulled off with tape. For these categories the standard allows a rating from 0 to 2. GALVANOL obtained 0 at the start, 2 after salt spray and 1 after humidity: within the requirement at all three points.

At what thickness

The dry film thickness was measured on each panel (ISO 2808). The averages were between 130 and 163 µm. This is the order of thickness we state in the technical data sheet for C4 very high and C5 high (from about 121 µm in 1-2 coats). With less thickness, the result would not be the same.

Laboratory conclusion

The samples meet the requirements of ISO 12944-6:2018 for C4 very high (more than 25 years) and C5 high (15 to 25 years), according to the durability ranges of ISO 12944-1.

Why the scribe doesn't rust

The most revealing figure is the 0 mm of corrosion creep from the scribe. With a barrier paint, rust gets in through the damage and creeps under the coat. With a coating with high zinc content, the zinc surrounding the cut sacrifices itself and protects the exposed steel. It is the same principle as hot-dip galvanizing, and that's why a knock or a scratch doesn't turn into a rust spot.

What it means and what it doesn't

ISO 12944 durability is a technical reference for choosing and specifying the system. It is not a warranty period. On site, real life also depends on surface preparation, applied thickness and maintenance.

Do you have a project in a C4 or C5 environment? We are the manufacturer: write to info@galvanol.eu and we'll help you define the thickness and system. Technical and safety data sheets are in Products.

 
 
 

Comments


Stay informed, subscribe to our newsletter

Thanks for subscribing!

bottom of page