Preventive maintenance of railway steel: the lesson of 2026
Updated: 3 hours ago
January 2026 will be remembered as one of the hardest months for Spanish railways. On 18 January, the derailment at Adamuz (Córdoba) cost 46 people their lives; two days later, at Gelida (Barcelona), a Rodalies commuter train hit a retaining wall that had collapsed in a storm. Our first thoughts are with the victims and their families.
Neither accident was caused by corrosion: at Adamuz the CIAF points to a rail break at a weld, and at Gelida to a wall collapsing during the storm. But both have raised the same question: are we caring for every element of the infrastructure as it deserves?
Maintenance moves to the forefront
The institutional response has been clear. In February 2026 Spain's Ministry of Transport and the rail unions agreed to increase maintenance investment by €1.8 billion and create 3,650 jobs over 2026-2030. More budget means more inspections, more maintenance contracts and higher demands on the quality of every repair.
Corrosion: the slow, silent enemy
Unlike a break, corrosion gives no sudden warning: it advances millimetre by millimetre at the base of a mast, under a nut or on an unprotected weld. NACE International's IMPACT study estimated that corrosion costs the world around US$2.5 trillion a year, roughly 3.4% of global GDP, and that applying good prevention practices could save between 15% and 35% of that cost.
On the railway, most track steel is galvanized and lasts for decades… as long as the zinc is still there. Problems start where the zinc is missing: installation cuts and drill holes, site welds, knocks, abrasion and bolts tightened after galvanizing.
Inspection checklist for galvanized track steel
Mast bases and anchor plates: water, mud and salts build up here. Look for red rust at the joint with the foundation.
Site welds and cuts: any weld made on site and left unrepaired is bare steel.
Fasteners: heads, nuts and washers, especially after adjustments or replacements.
Stairs, walkways and platforms: mechanical wear eats away the zinc on steps and railings.
Coastal and industrial sections (C4-C5): salt spray and pollutants speed up zinc consumption.
Warning signs: heavy white rust (the zinc is being consumed), brown stains and, above all, red rust (the steel is already under attack).
From warning to repair: act in time
Once red rust appears, the clock is ticking. The good news is that there is no need to dismantle the part or send it back to a galvanizing bath: the repair can be done on site with a zinc-rich cold galvanizing, as ISO 1461 and ASTM A780 provide for damaged galvanized areas.
GALVANOL has a minimum of 96% zinc in the dry film, is applied from −30 °C to +60 °C — ideal for night-time maintenance possessions — and achieved a C4 very high and C5 high classification in ISO 12944-6 tests. A minimum of 105 µm (4.1 mils) dry is recommended on structural elements.
A simple plan for maintenance teams
List the galvanized elements on each section and their corrosivity category (C3, C4, C5).
Inspect the critical points on the checklist at least once a year, and more often on the coast or in industrial areas.
Repair in the same intervention every new cut, weld or knock, rather than leaving it for the next campaign.
Measure the thickness of the repair with a gauge and record it.
Keep material in the vehicle: a tin of GALVANOL and a GALVANOL Spray let you repair on the spot.
To go further, read Corrosion on catenary masts and portals and GALVANOL for railways.
We help you prepare your plan
We are the manufacturer and work with electrification contractors, maintenance companies and railway engineering firms. We help you define thicknesses, consumption and formats for each campaign. Contact us at galvanol.eu/contacto, write to info@galvanol.eu or call +34 932 750 167 (WhatsApp +34 644 755 155).