Every day, millions of people trust that their train will reach its destination. That trust does not rest on the trains alone: it relies on thousands of tonnes of steel that hardly anyone looks at. Catenary masts and portals, cantilevers, signal supports, service stairs, walkways, railings, fences and fasteners hold the network up 24 hours a day, in rain, sun, frost and salt.

Almost all of that steel arrives on site hot-dip galvanized. But during installation and maintenance it is cut, drilled, welded and knocked, and at each of those points the zinc disappears and the steel is left bare. GALVANOL was created to restore that protection: a cold galvanizing with a minimum of 96% zinc, applied on site, with no furnaces and no dismantling.

2026: the year Spain looked at its infrastructure again

The accidents at Adamuz (18 January 2026, 46 deaths) and Gelida (20 January 2026) shocked the country. Neither had anything to do with corrosion: at Adamuz the CIAF investigation points to a rail break at a weld, and at Gelida a retaining wall fell onto the track during a storm. But both were a reminder of something every maintenance engineer knows: the safety of a network depends on every detail, including the ones you cannot see.

Since then, maintenance has moved to the forefront. In February 2026 Spain's Ministry of Transport agreed with the rail unions to increase maintenance investment by €1.8 billion and create 3,650 jobs up to 2030. For contractors, engineering firms and maintenance teams, that means more work, more inspections and higher quality demands on every repair.

Designed for all the galvanized steel on the line

  • Catenary masts and portals: installation cuts, drill holes and welds, and the critical area next to the base and anchor plates.

  • Cantilevers, stays and fittings: small parts that are adjusted on site and lose zinc with every intervention.

  • Signalling and communications supports: columns, masts, boxes and anchors exposed to the weather.

  • Service stairs, walkways and platforms: boots and tools wear the galvanizing away faster here than anywhere else.

  • Bridge and viaduct railings: humidity, de-icing salts and, on the coast, salt spray.

  • Station canopies, columns and fences: steel in full view of passengers, where rust shows too.

  • Perimeter fencing and fasteners: posts, mesh, gates, nuts and bolt heads after tightening.

Why zinc and not just any paint

Galvanizing protects in two ways: as a barrier and, above all, through cathodic protection: the zinc sacrifices itself so the steel does not rust. A conventional anti-corrosion paint is only a barrier; as soon as it is scratched, rust creeps in underneath. GALVANOL has a minimum of 96% zinc in the dry film (ISO 3549) and gives the repaired area the same active protection as the original galvanizing. That is why it complies as a galvanizing repair to ISO 1461 and ASTM A780.

And it is proven in harsh conditions: in tests to ISO 12944-6 at an accredited laboratory it passed 1,440 hours of salt spray and 720 hours of condensation with no blistering or rust and 0 mm corrosion creep from the scribe, with a classification of C4 very high and C5 high. In other words, suitable for coastal sections, industrial areas and places exposed to de-icing salts.

Made for the pace of railway work

  • Ready to use: single-component, no mixing; open, stir and apply.

  • For night-time possessions and winter: applied from −30 °C to +60 °C with up to 90% humidity.

  • Fast: touch-dry in about 20 minutes at 20 °C and dry in 4 hours.

  • A format for every job: tin and pail for surfaces; GALVANOL Spray for touching up bolts and welds.

  • Matching finish: accepts solvent-based topcoats, and ALINOL Spray gives the shine of new galvanizing.

For fixed infrastructure, not for the train

The EN 45545-2 standard and its fire requirements (R1, R3, R7…) apply to rolling stock: trains, coaches and trams. Fixed track steel is specified for corrosion (ISO 1461, ISO 12944, ASTM A780), and that is where GALVANOL works. We do not offer it for trains or vehicle interiors; in enclosed stations or tunnels, check the specification in case it sets additional requirements.

How to apply it in three steps

  1. Clean: remove rust, mill scale and slag down to clean metal (wire brush, disc or Sa 2½ blasting) and degrease.

  2. Apply in thin coats: first coat of about 60 µm (2.4 mils) and the following ones of 60–80 µm (3.1 mils), overlapping a few centimetres onto the sound galvanizing.

  3. Check the thickness: minimum 105 µm (4.1 mils) dry for structural repair (about 490 g/m²) and 69 µm (2.7 mils) on non-structural parts; full cure in 72 hours.

Let's make your network last for decades

If you work in electrification, track maintenance, engineering or railway structure manufacturing, we are the manufacturer and advise you directly: thickness, consumption and format for each project. Ask for prices or data sheets at galvanol.eu/contacto, write to info@galvanol.eu or call +34 932 750 167 (WhatsApp +34 644 755 155).

 
 
 