How to specify cold galvanizing in a technical specification

GALVANOL IBERIA SL
2 hours ago
2 min read
How to specify cold galvanizing in a technical specification

In many technical specifications, protection of repairs and welds is covered in one line: “apply zinc-rich paint”. With that wording almost any product qualifies, and not all of them protect equally. If you want the repair to last, specify data that can be checked.

1. Zinc content in the dry film

This is the key figure. What protects is the zinc left in the dry film, not what is in the can. Ask for the percentage in the dry film and the standard used to measure it. For example: “minimum 96 % zinc in the dry film per ISO 3549”, which GALVANOL meets.

2. Repair standards

For repairing hot-dip galvanizing, cite the reference standards: ISO 1461 and ASTM A780. State the repair thicknesses: 69 µm in non-structural areas and 105 µm in structural areas.

3. Durability by environment

Define the corrosivity category of the site per ISO 12944-2 and the durability you need. Then require an ISO 12944-6 test for that category and the thickness tested. With GALVANOL: 121 µm or more in C4 and 130 µm or more in 2 coats in C5, both for over 25 years. For CX, ISO 12944-9, a 2-coat system with at least 150 µm.

4. Surface preparation

  • SA 2½ blasting on new surfaces or with extensive rust.

  • Mechanical sanding with 180-220 grit for local repairs.

  • Degreasing beforehand in all cases.

5. Application conditions

State temperature and humidity limits and recoat times. With GALVANOL: application from −30 °C to +60 °C, maximum humidity 90 %, coats of 60-80 µm and a maximum total of 200 µm.

6. Inspection and documents

  1. Dry film thickness measurement per ISO 2808, with a sampling plan per ISO 19840.

  2. Product data sheet and safety data sheet.

  3. Manufacturer’s test reports (ISO 12944-6, conductivity ISO 787-14).

  4. Record of batches applied.

Sample clause

“Galvanizing repairs shall be carried out with a one-component cold galvanizing compound containing at least 96 % zinc in the dry film (ISO 3549), in accordance with ISO 1461 and ASTM A780, with a minimum dry film thickness of 105 µm on structural elements. The product shall have an ISO 12944-6 test for the site corrosivity category.”

If you are drafting a specification, we will send you the technical documents you need. You may also find our guide on how to read an ISO 12944-6 test report useful.

 
 
 