Power towers and substations: how to maintain galvanizing

Transmission towers, substation gantries and equipment supports are almost always made of hot-dip galvanized steel. It is excellent protection, but not eternal: zinc is consumed over the years, especially near the sea, in industrial areas and where water collects. When the coating is used up, red rust appears.
Where it fails first
Bolts and bolted joints, where the coating is thinner and moisture is retained.
Leg bases and areas close to the ground.
Cuts, drill holes and welds made during erection.
Knocks from transport and lifting.
Repair without dismantling
The great advantage of cold galvanizing is that it is applied in place, without dismantling and without taking parts to a bath. GALVANOL repairs galvanizing to ISO 1461 and ASTM A780: 69 µm in non-structural areas and 105 µm in structural areas. It can be applied from −30 °C to +60 °C, so work can continue in winter and in mountain areas.
Recharge the zinc before rust appears
When galvanizing starts to look dull and stained, there is still zinc, but not much. This is the best time to recharge: clean, remove loose white rust and apply a coat of cold galvanizing. This extends the life of the structure without reaching the red-rust stage, which requires much more costly preparation.
Reference thicknesses
C4 environment (ISO 12944-6): 121 µm or more, over 25 years.
C5 environment, for example coastal or heavy industry: 130 µm or more in 2 coats, over 25 years.
CX environment (ISO 12944-9): 2-coat system, minimum 150 µm.
Electrical safety
GALVANOL is conductive: it measures 0.0 Ω at 50 V and 1000 V (ISO 787-14). This keeps continuity between steel and zinc, which cathodic protection requires. Work on electrical installations must always follow the owner’s safety procedures, with isolation where required.
Recommended maintenance plan
Regular visual inspection, recording areas with white and red rust.
Immediate repair of erection damage with cold galvanizing, or with GALVANOL Spray on bolts.
Scheduled recharging of areas where galvanizing is used up.
Dry film thickness measurement after each intervention.
For maintenance plans on power networks, contact us and we will prepare a proposal.